Calorimetry, Differential Scanning

Synonyms

Calorimetric Differential Thermal Analysis

Differential Scanning Calorimetry

Differential Thermal Analysis, Calorimetric

Scanning Calorimetry, Differential

Differential thermal analysis in which the sample compartment of the apparatus is a differential calorimeter, allowing an exact measure of the heat of transition independent of the specific heat, thermal conductivity, and other variables of the sample.